| Authors | Abedini, M., Jahangiri, M.R., Karimi, P |
|---|---|
| Journal | Materials at High Temperatures |
| Paper Type | Full Paper |
| Published At | 2019 |
| Journal Grade | ISI |
| Journal Type | Typographic |
| Journal Country | Iran, Islamic Republic Of |
Abstract