CV
QR


Hossein Ashrafi

Hossein Ashrafi

Assistant Professor

College: Faculty of Mechanical Engineering

Department: Mechanical Engineering - Solid Design

Degree: Ph.D

CV
QR
Hossein Ashrafi

Assistant Professor Hossein Ashrafi

College: Faculty of Mechanical Engineering - Department: Mechanical Engineering - Solid Design Degree: Ph.D |

  •  Position: Assistant Professor of Solid Mechanics and Applied Design
  •  Institution: Faculty of Mechanical Engineering, University of Kashan, Iran
  •  Researcher ID: P-8090-2014
  •  Scopus Author ID: 12793997500
  •  M.Sc. (Sept. 2005 – August 2008): Graduated from Shiraz University, with Overall GPA 17.67 out of 20.
  •  Ph.D. (Sept. 2010 – August 2014): Graduated from K.N. Toosi University, with Overall GPA 19.43 out of 20.
  • Address: No. 316, 3rd Floor, Faculty of Mech. Eng., University of Kashan, Ghotbravandi Blvd., Kashan, Iran
  • ​P.O. Box:  8731751167
  • Telephone:  (+98) 31 55913439
  • Fax:  (+98) 31 55913444
  • URL:  https://faculty.kashanu.ac.ir/hashrafi/en​

 

نمایش بیشتر

A Nanoindentation Modeling of Viscoelastic Creep and Relaxation Behaviors of Ligaments, mechanical characteristics of biological tissues

AuthorsH Ashrafi - M Shariyat
Conference TitleIEEE 17th Iranian Conference on Biomedical Engineering
Holding Date of Conference2010-11-3
Event Placeاصفهان
PresentationSPEECH
Conference LevelInternational Conferences

Abstract

Nanoindentation has recently appeared as a powerful tool for measuring nano and micro-scale mechanical properties of biological tissues. In biological engineering, the majority of soft tissues exhibit as viscoelastic materials with a time-dependent response. However, the viscoelastic constitutive effects of biological tissues during nanoindentation are seldom considered rigorously. The presented paper develops a mathematical contact approach for independently measuring of creep compliance and relaxation modulus of periodontal ligaments from nanoindentation tests using the constant – rate displacement and loading histories, respectively. A proper curve – fitting method has been developed to measure these characteristics via the nanoindentation of rigid Berkovich tips. Generalized Voigt-Kelvin and Wiechert models have been used to model constitutive equations of ligaments, in which relaxation and creep functions are represented by sum of a series of decaying exponential functions of time. Relaxation and Creep moduli should be measured from two nanoindentation tests separately to improve accuracy. Stress relaxation proceeds more rapidly than creep in periodontal ligaments.