| Authors | H Ashrafi - S Madadi |
|---|---|
| Conference Title | 1st International Conference on Rheology (ICOR) |
| Holding Date of Conference | 2019/12/17 |
| Event Place | Amirkabir University of Technology |
| Presented by | بلی |
| Presentation | SPEECH |
| Conference Level | International Conferences |
Abstract
| The objective of this study is to develop a general augmented Lagrangian finite element formulation associated with an incremental adaptive procedure which established for the frictional viscoelastic contact analysis of Nano indentation on solid films. For modeling the viscoelastic constitutive equations, a general Wiechert model has been used |