CV


FA
Hossein Ashrafi

Hossein Ashrafi

Assistant Professor

College: Faculty of Mechanical Engineering

Department: Mechanical Engineering - Solid Design

Degree: Ph.D

CV
FA
Hossein Ashrafi

Assistant Professor Hossein Ashrafi

College: Faculty of Mechanical Engineering - Department: Mechanical Engineering - Solid Design Degree: Ph.D |

  •  Position: Assistant Professor of Solid Mechanics and Applied Design
  •  Institution: Faculty of Mechanical Engineering, University of Kashan, Iran
  •  Researcher ID: P-8090-2014
  •  Scopus Author ID: 12793997500
  •  M.Sc. (Sept. 2005 – August 2008): Graduated from Shiraz University, with Overall GPA 17.67 out of 20.
  •  Ph.D. (Sept. 2010 – August 2014): Graduated from K.N. Toosi University, with Overall GPA 19.43 out of 20.
  • Address: No. 316, 3rd Floor, Faculty of Mech. Eng., University of Kashan, Ghotbravandi Blvd., Kashan, Iran
  • ​P.O. Box:  8731751167
  • Telephone:  (+98) 31 55913439
  • Fax:  (+98) 31 55913444
  • URL:  https://faculty.kashanu.ac.ir/hashrafi/en​

 

Show More

Modeling of viscoelastic properties for polymeric thin solid layers using a contact nanoindentation approach

AuthorsAshrafi, H. Shariyat, M
JournalIranian Journal of Surface Science and Engineering
Page number 17-26
Volume number۸
Paper TypeOriginal Research
Published At۲۰۱۲
Journal GradeScientific - research
Journal TypeTypographic
Journal CountryIran, Islamic Republic Of

Abstract

Paper URL